Duplex stainless steels are widely used in industrial sectors characterized by aggressive environments due to their combination of high mechanical properties and good corrosion resistance at a reasonable cost. However, exposure to heat treatments in the 750°C to 900°C temperature range can promote the precipitation of secondary phases, resulting in changes to the material's microstructure and performance. The aim of this study is to evaluate the influence of isothermal aging on the corrosion resistance and mechanical characteristics of 2205 duplex stainless steel. To this end, various samples of the material were heated to 750°C, 800°C, 850°C and 900°C for a holding time of one and three hours, water-quenched, and polished in preparation for testing. Corrosion resistance was investigated using Potentiodynamic Polarization (PDP) and Double Loop Electrochemical Potentiodynamic Reactivation (DL-EPR) tests. Local mechanical properties were characterized via Vickers microhardness measurements. Finally, the samples were examined using an optical microscope; modified Beraha II reagent and a 40% sodium hydroxide solution were used to reveal the microstructure. The results highlight how increasing the treatment temperature promotes the material's microstructural evolution, affecting both corrosion behavior and mechanical properties. PDP analyses show a variation in corrosion resistance in samples treated at higher temperatures. DL-EPR tests indicate an increase in the degree of sensitization, attributable to the formation of precipitates and the consequent local depletion of alloying elements in adjacent zones. At the same time, Vickers microhardness measurements reveal an increase in hardness following heat treatment, linked to the presence of newly precipitated phases. However, the low volume fraction of these phases renders this particular test relatively insensitive. The study confirms that heat treatments in the 750°C - 900°C range significantly affect the performance of 2205 duplex steel, resulting in a trade-off between increased hardness and reduced corrosion resistance.

Gli acciai inossidabili duplex sono ampiamente impiegati in settori industriali caratterizzati da ambienti aggressivi grazie alla loro combinazione di elevate proprietà meccaniche e buona resistenza alla corrosione a un costo mantenuto. Tuttavia, l’esposizione a trattamenti termici nell’intervallo di temperatura compreso tra 750 °C e 900 °C può favorire la precipitazione di fasi secondarie, con conseguenti modifiche della microstruttura e delle prestazioni del materiale. Lo scopo di questo studio è valutare l’influenza dell’invecchiamento isotermo sulla resistenza alla corrosione e sulle caratteristiche meccaniche dell’acciaio inox duplex 2205. A tal fine, vari campioni del materiale sono stati riscaldati a 750 °C, 800 °C, 850 °C e 900 °C per un tempo di permanenza di 1 e 3 ore, raffreddati in acqua e lucidati per poter compiere su di loro i vari test. La resistenza alla corrosione è stata investigata mediante prove di Polarizzazione Potenziodinamica (PDP) e Double Loop Electrochemical Potentiodinamic Reactivation (DL-EPR). Le proprietà meccaniche locali sono state invece caratterizzate attraverso misure di microdurezza Vickers. I campioni sono stati infine osservati al microscopio ottico e, per mettere in evidenza la microstuttura, sono stati usati i reagenti Beraha II modificato e una soluzione di idrossido di sodio al 40%. I risultati evidenziano come l’aumento della temperatura di trattamento favorisca l’evoluzione microstrutturale del materiale, con effetti sul comportamento corrosivo e sulle proprietà meccaniche. Le analisi PDP mostrano una variazione della resistenza alla corrosione nei campioni trattati alle temperature più elevate. I test DL-EPR indicano un aumento del grado di sensibilizzazione, attribuibile alla formazione di precipitati e al conseguente impoverimento locale di elementi leganti nelle zone adiacenti. Parallelamente, le misure di microdurezza Vickers evidenziano un incremento della durezza in seguito ai trattamenti termici, correlato alla presenza delle nuove fasi precipitate. Tuttavia, l'esigua percentuale in volume di queste fasi rendono quest'ultimo test poco sensibile. Lo studio conferma che i trattamenti termici nell’intervallo 750 °C - 900 °C influenzano in modo significativo le prestazioni dell’acciaio duplex 2205, determinando un compromesso tra incremento della durezza e riduzione della resistenza alla corrosione.

Effetti dell'invecchiamento isotermo sulla resistenza alla corrosione e sulle proprietà meccaniche dell'acciaio inox duplex 2205

FARINOLA, FILIPPO
2025/2026

Abstract

Duplex stainless steels are widely used in industrial sectors characterized by aggressive environments due to their combination of high mechanical properties and good corrosion resistance at a reasonable cost. However, exposure to heat treatments in the 750°C to 900°C temperature range can promote the precipitation of secondary phases, resulting in changes to the material's microstructure and performance. The aim of this study is to evaluate the influence of isothermal aging on the corrosion resistance and mechanical characteristics of 2205 duplex stainless steel. To this end, various samples of the material were heated to 750°C, 800°C, 850°C and 900°C for a holding time of one and three hours, water-quenched, and polished in preparation for testing. Corrosion resistance was investigated using Potentiodynamic Polarization (PDP) and Double Loop Electrochemical Potentiodynamic Reactivation (DL-EPR) tests. Local mechanical properties were characterized via Vickers microhardness measurements. Finally, the samples were examined using an optical microscope; modified Beraha II reagent and a 40% sodium hydroxide solution were used to reveal the microstructure. The results highlight how increasing the treatment temperature promotes the material's microstructural evolution, affecting both corrosion behavior and mechanical properties. PDP analyses show a variation in corrosion resistance in samples treated at higher temperatures. DL-EPR tests indicate an increase in the degree of sensitization, attributable to the formation of precipitates and the consequent local depletion of alloying elements in adjacent zones. At the same time, Vickers microhardness measurements reveal an increase in hardness following heat treatment, linked to the presence of newly precipitated phases. However, the low volume fraction of these phases renders this particular test relatively insensitive. The study confirms that heat treatments in the 750°C - 900°C range significantly affect the performance of 2205 duplex steel, resulting in a trade-off between increased hardness and reduced corrosion resistance.
2025
Effects of isothermal aging on corrosion behaviour and mechanical properties of duplex stainless steel 2205
Gli acciai inossidabili duplex sono ampiamente impiegati in settori industriali caratterizzati da ambienti aggressivi grazie alla loro combinazione di elevate proprietà meccaniche e buona resistenza alla corrosione a un costo mantenuto. Tuttavia, l’esposizione a trattamenti termici nell’intervallo di temperatura compreso tra 750 °C e 900 °C può favorire la precipitazione di fasi secondarie, con conseguenti modifiche della microstruttura e delle prestazioni del materiale. Lo scopo di questo studio è valutare l’influenza dell’invecchiamento isotermo sulla resistenza alla corrosione e sulle caratteristiche meccaniche dell’acciaio inox duplex 2205. A tal fine, vari campioni del materiale sono stati riscaldati a 750 °C, 800 °C, 850 °C e 900 °C per un tempo di permanenza di 1 e 3 ore, raffreddati in acqua e lucidati per poter compiere su di loro i vari test. La resistenza alla corrosione è stata investigata mediante prove di Polarizzazione Potenziodinamica (PDP) e Double Loop Electrochemical Potentiodinamic Reactivation (DL-EPR). Le proprietà meccaniche locali sono state invece caratterizzate attraverso misure di microdurezza Vickers. I campioni sono stati infine osservati al microscopio ottico e, per mettere in evidenza la microstuttura, sono stati usati i reagenti Beraha II modificato e una soluzione di idrossido di sodio al 40%. I risultati evidenziano come l’aumento della temperatura di trattamento favorisca l’evoluzione microstrutturale del materiale, con effetti sul comportamento corrosivo e sulle proprietà meccaniche. Le analisi PDP mostrano una variazione della resistenza alla corrosione nei campioni trattati alle temperature più elevate. I test DL-EPR indicano un aumento del grado di sensibilizzazione, attribuibile alla formazione di precipitati e al conseguente impoverimento locale di elementi leganti nelle zone adiacenti. Parallelamente, le misure di microdurezza Vickers evidenziano un incremento della durezza in seguito ai trattamenti termici, correlato alla presenza delle nuove fasi precipitate. Tuttavia, l'esigua percentuale in volume di queste fasi rendono quest'ultimo test poco sensibile. Lo studio conferma che i trattamenti termici nell’intervallo 750 °C - 900 °C influenzano in modo significativo le prestazioni dell’acciaio duplex 2205, determinando un compromesso tra incremento della durezza e riduzione della resistenza alla corrosione.
Acciaio
Duplex
Corrosione
Microdurezza
Attacco chimico
File in questo prodotto:
File Dimensione Formato  
Farinola_Filippo.pdf

Accesso riservato

Dimensione 1.72 MB
Formato Adobe PDF
1.72 MB Adobe PDF

The text of this website © Università degli studi di Padova. Full Text are published under a non-exclusive license. Metadata are under a CC0 License

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.12608/115364